Spunbond nonwoven fabric is the behind-the-scenes hero of medical gowns, grocery bags, and many other applications. As an ISO 9001 certified nonwoven fabric manufacturer, we've been producing more than 50 million square meters of spunbond fabric annually for global customers. In this guide, we pull back the curtain on the making of spunbond nonwoven fabric-from polymer pellets to finished rolls-and give you the inside scoop on quality control, machinery, and environmental innovations.

How Spunbond Nonwoven Fabric Is Made Step-By-Step From The Manufacturer

Spunbond nonwoven fabric is created from
Spunbond nonwoven fabric is a lightweight, strong material created by bonding continuous filaments of thermoplastic polymer (such as polypropylene) using heat and pressure. In comparison to woven fabrics, it bypasses the yarn-spinning step, providing benefits such as:

Cost Effectiveness: 30–50% lower cost than woven

Customization features are adjustable weight (10–150 gsm), color, and additives (e.g., UV

Sustainability: 100% recyclable (being increasingly used in circular packaging

 

Raw Materials are the Pillars of Quality
1. Polymer Selection
Polypropylene (PP): 85% of spunbond fabrics use PP due to its chemical resistance and stability upon melting.

Polyester (PET): For high temperature applications (e.g.,

Additives

Antistatic agents: For electronics packaging.

Hydrophilic agents: Liquid absorption facilitation (medical textiles

Pro Tip: Food-grade spunbond needs FDA-approved polymers (21 CFR 177.1520

 

Step 1: Polymer Extrusion
Process
Drying: PP raw pellets are dried at 80–100°C to evaporate the moisture (prevents bubble formation).

Melting: Pellets are fed to an extruder and melted at 220–250°C.

Filtration: The polymer is filtered through 20–50 μm filter to remove impurities.

Equipment: Single screw extruders (for regular fabrics) versus twin screw (for composite material).

 

Step 2: Filament Spinning
Major Milestones
Spinneret: The polymer is pushed through a spinneret plate having 1,000–4,000 holes (0.2–0.4 mm diameter

Quenching: High-speed air (20–25 m/s) is used to cool hot filaments and freeze

Drawing: Molecules are aligned by stretching filaments, enhancing tensile strength.

Critical Parameters

Air pressure: 0.3–0.5 MPa for constant fiber diameter (1–

Throughput: 0.5–1.5 grams per hole per minute

 

Step 3: Web Formation
Filaments are randomly deposited onto a conveyor belt by one of two methods:

A. Aerodynamic web forming
How It Works: Air turbulence spreads filaments to create an even web.

Benefit: Creates softer fabrics (best suited for hygiene products).

B. Mechanical Layering
How It Works: Stacking multiple filament layers to produce thicker fabrics (e.g., 100+ gsm).

Benefit: Up to 500 m/min faster production speeds.

Fault Alert: Unbalanced webs produce weak spots-real-time cameras check gaps as they are created.

 

Step 4: Bonding
This step determines the fabric's strength and texture.

A. Thermal Bonding (Most Common)
1.Calendering: The web is taken through hot rolls (140–160°C) that melt the fibers upon contact.

Roller Patterns

Diamond/square bond patterns (20–40% bond area

Smooth Roll: Creates very soft fabrics (diapers).

 

2.Through-Air Bonding: Hot air (200°C) bonds the entire web (higher loft, lower strength).

 

B. Chemical bonding
Used For: Heavy-duty fabrics (geotextiles).

Process: Spraying acrylic binders and drying ovens.

 

Step 5: Finishing Treatments
1. Hydroent
Fibers are entangled under high pressure to achieve extra softness (spunlace method).

Applications: Surgical drapes and wet wipes.

 

2. Coating
Examples

PE Coating: Waterproofing Disposable Aprons

Antimicrobial Layer: For medical textiles (tested as per AATCC 100).

 

3. Slitting and Winding
It is trimmed to 1–5 meter widths and wrapped around 3,000–5,000 meter rolls.

 

Quality Control: Industry Secrets

1. Laboratory Tests

Tensile Strength: ASTM D5034 (min 25 N/5cm on 50

Air Permeability: ASTM D737 (most relevant to face mask fabrics).

Hydrostatic pressure: AATCC 127 (waterproof fabrics

 

2. On-Line Monitoring

X-ray sensors detect impurities as minute as 0.1 mm.

Basis Weight Gauges: Monitor ±2% uniformity between rolls.

Case Study: A European client rejected 10% of shipments due to uneven weight-resolved by upgrading to laser-guided sensors.

 

Sustainability in Spunbond Production

1. Recycling Materials

Post-industrial PP waste can replace 30–50% of virgin polymer (GRS certified).

Challenge: 15–20% weaker tensile strength are recycled fibers.

 

2. Energy Efficiency

Recovery systems recycle 40% of thermal energy from extruders.

Our solar-powered plants reduce carbon footprint by 25%.

 

3. End-of-Life Solutions

Take-back programs for used nonwovens (reprocessed into automotive insulation).


Applications of Spunbond Nonwoven Fabric

Industry Use Case Key Requirements
Medical Surgical gowns ISO 13485, AAMI Level 3 barrier
Agriculture Crop covers UV-resistant, 80+ gsm
Packaging Shopping bags 70–90 gsm, 20% recycled content
Construction Roofing membranes Fire-retardant (EN 13501-1)
FAQ

Q: Can spunbond fabric be sterilized for medical use?

A: Yes--gamma radiation or ethylene oxide (ETO) sterilization are common.

Q: What is the MOQ for spunbond custom-width?

A: Typically 5 tons, although we take trial orders of 1 ton from new customers.

Q: How does spunbond compare to meltblown fabric?

A: Spunbond has higher strength; meltblown offers better filtration (often used in composites).

Q: Can you add logos to spunbond rolls?

A: Yes-custom embossing or dye-sublimation printing (min. 10,000m run).

Why Choose Our Spunbond Nonwoven Fabric?

40+ Configurations: From 10 gsm lightweight to 150 gsm reinforced.

Certifications: ISO 9001, OEKO-TEX® Standard 100, FDA-compliant.

Fast Turnaround: 15-day production + 7-day shipping via bonded warehouses.